Journal of Textile Research ›› 2025, Vol. 46 ›› Issue (10): 1-10.doi: 10.13475/j.fzxb.20241202201

• Fiber Materials •     Next Articles

Simulation of devolatilization and viscosity increase reaction of polyamide 6 falling film for direct melt spinning

CHEN Shichang1,2(), LOU Shunyue1,2, CHEN Wenxing1   

  1. 1. National Engineering Laboratory for Textile Fiber Materials Processing Technology, Zhejiang Sci-Tech University, Hangzhou, Zhejiang 310018, China
    2. Zhejiang Provincial Innovation Center of Advanced Textile Technology, Shaoxing, Zhejiang 312000, China
  • Received:2024-12-10 Revised:2025-04-19 Online:2025-10-15 Published:2025-10-15

Abstract:

Objective In view of the current situation of long chip spinning production process and high energy consumption in the production of polyamide 6(PA6), a process simulation analysis was conducted on the preparation of low-volatile polyamide 6 melt. By adding a falling film devolatilization reactor with vacuum facility after two-stage polymerization, multiple systems such as cooling granulation, hot water extraction, drying, solid phase adhesion and extrusion melting could be eliminated to realize the direct spinning of polyamide 6 fiber.

Method The outlet data of polyamide 6 two-stage VK tube established in Polymer Plus is taken as the inlet parameter of the falling film devolatilization reactor. The mathematical model established according to reaction kinetics, mass transfer and material balance is essentially a set of partial differential equations. MatLab is used to calculate the devolatilization and viscosity increase process of the falling film devolatilization reactor. When the reactor operation reaches a steady state, the concentration of each component in the reactor no longer changes with the change of time, and the concentration of the main component at the liquid phase outlet of the devolatilizing reactor and related technical indicators are obtained.

Results The model investigated the effects of different melt feed parameters, reaction temperature, pressure and other factors on the number average molecular weight (Mn), extractable content and end group concentration during the viscosity increasing process of falling film reactor. The results showed that high temperature and low pressure improved the performance of the product, but too low pressure caused costs increase for industrial production, making it more difficult to control. The by-products in high-temperature products tended to increase, which is not conducive to subsequent spinning. The results suggested that when the relative viscosity (ηr) of inlet melt was increased, the ηr of polymer increased slowly with the increase of reactor length, and the contents of monomer caprolactam (mCPL) and oligomer (CO) decreased gradually. When the reaction temperature of the falling film reactor was increased, the Mn of polyamide 6 melt gradually increased, while mCPL and CO gradually decreased. When the pressure of the reactor was reduced, the Mn gradually increased, and the mCPL and CO gradually decreased. Therefore, the process parameters of 260 ℃ and 200 Pa were selected to obtain a high viscosity polymer with a Mn of 21 709 g/mol, monomer content (mCPL) of 0.230%, and oligomer content (CO) of 0.115%.

Conclusion When the ηr of inlet material increases, the ηr of melt decreases with the increase of falling film flow distance, and the mCPL and CO decrease gradually. After the melt with a ηr of 2.35 passes through the falling film devolatilization reactor, its ηr can be increased to 3.1. The effects of reaction temperature, pressure and other conditions on polymer number, Mn, ηr, mCPL, CO and end group concentration in falling film devolatilization reactor were studied. With the increase of reaction temperature, the Mn of polymers in a certain range increased linearly, the mCPL decreased from 7.062% to 0.230%, the CO decreased from 0.710% to 0.115%, and the end group concentration([NH2] and [COOH]) also decreased gradually. By controlling the pressure of the falling film devolatilization reactor, it is shown that the relative viscosity of the polymer is improved at low pressure. Reduce the mCPL and CO in melt. By adjusting and controlling the inlet melt parameters of the falling film devolatilization reactor, high quality PA6 melt can be obtained under suitable devolatilization reaction temperature and vacuum degree. The research results are conducive to the development of direct spinning technology of PA6 melt.

Key words: polyamide 6, relative viscosity, falling film reactor, devolatilization, process simulation, direct melt spinning

CLC Number: 

  • TQ342.1

Fig.1

Production process of polyamide 6 fiber"

Tab.1

Simulation results of polyamide 6 two-stage polymerization"

参数 目标值 模拟值
数均分子量Mn 12 000~15 000 g/mol 14 538 g/mol
相对黏度ηr 2.100~2.400 2.350
端胺基初始浓度[NH2] 45.634 mmol/kg
端羧基初始浓度[COOH] 62.228 mmol/kg
水初始浓度[H2O] 60.088 mmol/kg
己内酰胺质量分数mCPL 7.000%~9.000% 7.060%
低聚物O质量分数CO 0.080%~2.000% 0.710%

Fig.2

Plug flow model of falling film reactor flow"

Tab.2

Mechanism of devolatilization of polyamide 6"

反应编号 反应方程式
S1 $\mathrm{P}_{1}+\mathrm{P}_{1} \underset{k_{1} / K_{1}}{\stackrel{k_{1}}{\rightleftharpoons}} \mathrm{COOH}-\mathrm{NH}_{2}+\mathrm{H}_{2} \mathrm{O}$
S2 $\mathrm{NH}_{2}+\mathrm{COOH} \underset{k_{1} / K_{1}}{\stackrel{k_{1}}{\rightleftharpoons}} \mathrm{~B} \_\mathrm{ACA}-\mathrm{B} \_\mathrm{ACA}+\mathrm{H}_{2} \mathrm{O}$
S3 $\mathrm{P}_{1}+\mathrm{COOH} \underset{k_{1} / K_{1}}{\stackrel{k_{1}}{\rightleftharpoons}} \mathrm{COOH}-\mathrm{B} \_\mathrm{ACA}+\mathrm{H}_{2} \mathrm{O}$
S4 $\mathrm{P}_{1}+\mathrm{NH}_{2} \underset{\overline{k_{1} / K_{1}}}{\stackrel{k_{1}}{\rightleftharpoons}} \mathrm{NH}_{2}-\mathrm{B} \_\mathrm{ACA}+\mathrm{H}_{2} \mathrm{O}$
S5 $\mathrm{CPL}+\mathrm{H}_{2} \mathrm{O} \underset{k_{2} / K_{2}}{\stackrel{k_{2}}{\rightleftharpoons}} \mathrm{P}_{1}$
S6 $\mathrm{P}_{1}+\mathrm{CPL} \underset{k_{3} / K_{3}}{\stackrel{k_{3}}{\rightleftharpoons}} \mathrm{NH}_{2}-\mathrm{COOH}$
S7 $\mathrm{NH}_{2}+\mathrm{CPL} \underset{k_{3} / K_{3}}{\stackrel{k_{3}}{\rightleftharpoons}} \mathrm{NH}_{2}-\mathrm{B} \_\mathrm{ACA}$
S8 $\mathrm{O}+\mathrm{H}_{2} \mathrm{O} \underset{\overline{k_{4} / K_{4}}}{\stackrel{k_{4}}{\rightleftharpoons}} \mathrm{COOH}-\mathrm{NH}_{2}$
S9 $\mathrm{O}+\mathrm{P}_{1} \underset{k_{5} / K_{5}}{\stackrel{k_{5}}{\rightleftharpoons}} \mathrm{COOH}-\mathrm{B} \_\mathrm{ACA}-\mathrm{NH}_{2}$
S10 $\mathrm{O}+\mathrm{NH}_{2} \underset{k_{5} / K_{5}}{\stackrel{k_{5}}{\rightleftharpoons}} \mathrm{~B} \_\mathrm{ACA}-\mathrm{B} \_\mathrm{ACA}-\mathrm{NH}_{2}$

Fig.3

Distribution of components outside tube of falling film devolatilization reactor. (a)ηr and Mn; (b)[NH2] and [COOH]; (c)QCPL and Q H 2 O"

Fig.4

Variation of melt parameters along reactor axis at different feed initial relative viscosities"

Fig.5

Variation of Mn along reactor axis at different temperatures"

Fig.6

Component concentration along reactor axis at different temperatures"

Fig.7

Variation of Mn along reactor axis at different pressure"

Fig.8

Component concentration along reactor axis at different pressure"

[1] 李睿, 王梦柯, 于春晓, 等. 原位聚合法聚酰胺6/炭黑复合纤维的制备及其性能[J]. 纺织学报, 2023, 44(10): 1-8.
doi: 10.13475/j.fzxb.20220505601
LI Rui, WANG Mengke, YU Chunxiao, et al. Fabrication and properties of polyamide 6/carbon black composite fibers via in situ polymerization[J]. Journal of Textile Research, 2023, 44(10): 1-8.
doi: 10.13475/j.fzxb.20220505601
[2] ČOLOVIĆ M, VASILJEVIĆ J, ŠTIRN Ž, et al. New sustainable flame retardant DOPO-NH-functionalized polyamide 6 and filament yarn[J]. Chemical Engineering Journal, 2021, 426: 130760.
doi: 10.1016/j.cej.2021.130760
[3] WANG L, GUO Z X, YU J. Effect of glass fibers with different surface properties on the morphology and properties of polyamide 6/poly(butylene terephthalate) blends[J]. Industrial & Engineering Chemistry Research, 2014, 53(1): 206-213.
doi: 10.1021/ie4026133
[4] 范学松, 张圣明, 王朝生, 等. 己内酰胺聚合中低聚物控制及PA6熔体直纺可行性研究[J]. 合成纤维工业, 2020, 43(5): 1-6.
FAN Xuesong, ZHANG Shengming, WANG Chaosheng, et al. Study on oligomer control during caprolactam hydrolytic polymerization and feasibility of PA6 melt direct spinning[J]. Synthetic Fiber Industry, 2020, 43(5): 1-6.
[5] FANG H, SU S, LUO Y, et al. Unveiling the mechanisms of hydrolytic ring-opening polymerization of caprolactam and amino-assisted ring opening of cyclic dimers: a DFT study[J]. Industrial & Engineering Chemistry Research, 2023, 62(1): 136-144.
doi: 10.1021/acs.iecr.2c03328
[6] ZHANG S, MENG C, WU Y, et al. Efficient production of copolymerized PA6-based polymer fibers: oligomer control and direct melt spinning[J]. Polymer, 2024, 296: 126762.
doi: 10.1016/j.polymer.2024.126762
[7] 陈文兴, 马建平, 王建辉, 等. 涤纶工业丝熔体直纺生产技术的研发[J]. 合成纤维工业, 2013, 36(4): 1-4.
CHEN Wenxing, MA Jianping, WANG Jianhui, et al. Development of melt direct spinning process technology for polyester industrial yarn[J]. Synthetic Fiber Industry, 2013, 36(4): 1-4.
[8] YUAN W, MA J, CHEN S. Surface renewal and residence time distribution of highly viscous liquid falling film flow[J]. Theoretical Foundations of Chemical Engineering, 2023, 57(6): 1414-1423.
doi: 10.1134/S0040579523060209
[9] CHEN S, CHEN S, GUANG S, et al. Film reaction kinetics for melt post polycondensation of poly(ethylene terephthalate)[J]. Journal of Applied Polymer Science, 2020, 137(34): 48988.
doi: 10.1002/app.v137.34
[10] 陈世昌, 曹峻华, 陈文兴. 聚酯降膜增黏反应过程模拟[J]. 纺织学报, 2025, 46(1): 16-24.
CHEN Shichang, CAO Junhua, CHEN Wenxing. Process simulation of falling film liquid-state polycondensation of polyester[J]. Journal of Textile Research, 2025, 46(1): 16-24.
[11] 赵玲, 邢玉林, 秦春曦, 等. 尼龙6连续聚合过程的流程模拟和调控[J]. 化学反应工程与工艺, 2014, 30(6): 481-490.
ZHAO Ling, XING Yulin, QIN Chunxi, et al. Simulation and control of nylon-6 continuous polymerization process[J]. Chemical Reaction Engineering and Technology, 2014, 30(6): 481-490.
[12] SEAVEY K C, KHARE N P, LIU Y A, et al. A new phase-equilibrium model for simulating industrial nylon-6 production trains[J]. Industrial & Engineering Chemistry Research, 2003, 42(17): 3900-3913.
doi: 10.1021/ie030112+
[13] GUPTA S K, KUMAR A, AGRAWAL K K. Simulation of three-stage nylon 6 reactors with intermediate mass transfer at finite rates[J]. Journal of Applied Polymer Science, 1982, 27(8): 3089-3101.
doi: 10.1002/app.07.v27:8
[14] CHEN S, ZHANG L, WANG Y, et al. Residence time distribution of high viscosity fluids falling film flow down outside of industrial-scale vertical wavy wall: experimental investigation and CFD prediction[J]. Chinese Journal of Chemical Engineering, 2019, 27(7): 1586-1594.
doi: 10.1016/j.cjche.2018.12.022
[15] 商利容, 王健红. PET聚合反应器建模及在聚合流程动态模拟中的应用[J]. 计算机仿真, 2003, 20(2): 99-102.
SHANG Lirong, WANG Jianhong. Modeling of poly(ethylene terephthalate) reactor and its application in the dynamic simulation of polymerization process[J]. Computer Simulation, 2003, 20(2): 99-102.
[16] SEAVEY K C, LIU Y A, LUCAS B, et al. New mass transfer model for simulating industrial nylon-6 production trains[J]. Industrial & Engineering Chemistry Research, 2004, 43(17): 5063-5076.
doi: 10.1021/ie040067l
[17] XIAO W, HUANG N, TANG Z, et al. Simulation of nylon 6 polymerization in an industrial two-step VK tubular reactor[J]. Macromolecular Materials and Engineering, 2003, 288(3): 235-244.
doi: 10.1002/mame.v288:3
[18] NAGASUBRAMANIAN K, REIMSCHUESSEL H K. Diffusion of water and caprolactam in nylon 6 melts[J]. Journal of Applied Polymer Science, 1973, 17(6): 1663-1677.
doi: 10.1002/app.07.v17:6
[19] NASR A, SVOBODA P. Influence of fusion temperature on nonisothermal crystallization kinetics of polyamide 6[J]. Polymers, 2023, 15(8): 1952.
doi: 10.3390/polym15081952
[20] ZHANG S, WU Y, JI P, et al. Sustainable production of polyamide 6 fibers: direct melt spinning and efficient reuse of residual oligomers during polymerization[J]. ACS Sustainable Chemistry & Engineering, 2023, 11(9): 3789-3800.
[21] CHEN S, ZHONG S, CHEN W. Kinetics comparison of solid-state polycondensation and melt post polycondensation for polyamide 6 with controllable extractive content[J]. Industrial & Engineering Chemistry Research, 2024, 63(22): 9740-9750.
doi: 10.1021/acs.iecr.4c00744
[22] ZHONG S, GUO Y, GAO F, et al. Studies of caprolactam and cyclic oligomer content, molecular weight, and thermal properties during melt post-polycondensation of polycaprolactam in the film state[J]. Polymer, 2023, 27: 125802.
[1] LI Jian'ge, WU Wei, HAN Weipeng, JI Bolin, XU Hong, MAO Zhiping. Synthesis of new ethylene sulfone acetate reactive disperse dyes and its dyeing performance for polyamide 66 fabrics [J]. Journal of Textile Research, 2025, 46(10): 143-151.
[2] LI Yujie, WANG Chengqin, WANG Wei, YUAN Ruchao, YU Jianyong, LI Faxue. Fabrication and properties of polyamide 6-based elastomers and their side-by-side elastic fibers [J]. Journal of Textile Research, 2025, 46(09): 46-56.
[3] MA Chaohui, CUI Tongran, BING Linhan, ZHU Zhiguo, WANG Rui, WEI Jianfei. Optimization of preparation technology for polyethylene terephthalate-based carbom dots and its application in polyamide 66 [J]. Journal of Textile Research, 2025, 46(08): 28-36.
[4] LIAO Mengdie, XIAO Wangyang, LI Hongxin, ZHAO Man, ZHANG Xuzhen, WANG Xiuhua. Preparation and properties of polyamide 6/copolyamide eccentric sheath-core composite fibers [J]. Journal of Textile Research, 2025, 46(07): 53-61.
[5] WANG Zihan, LI Yong, CHEN Xiaochuan, WANG Jun, LIANG Lingjie. Modeling and simulation of waste cotton fabric shredding process [J]. Journal of Textile Research, 2025, 46(07): 136-143.
[6] CHEN Yajuan, GUO Hanyu, ZHANG Chentian, LI Xinxin, ZHANG Xueping. Preparation and hygroscopic properties of polyvinyl alcohol/sodium alginate/polyamide 66 composite hydrogel core-spun yarns [J]. Journal of Textile Research, 2025, 46(06): 103-110.
[7] CHEN Shichang, CAO Junhua, CHEN Wenxing. Process simulation of falling film liquid-state polymerization of polyester [J]. Journal of Textile Research, 2025, 46(01): 16-24.
[8] XU Qiuge, GUO Xun, DUO Yongchao, WU Ruonan, QIAN Xiaoming, SONG Bing, FU Hao, ZHAO Baobao. Preparation and performance of high shrinkage polyester/polyamide 6 hollow pie-segmented spunbond needle-punching nonwovens [J]. Journal of Textile Research, 2024, 45(12): 41-49.
[9] DENG Gang, ZHANG Tao, WU Chaoping, WANG Jun, ZHANG Lei. Simulation of dry spinning process and cross-section analysis of profiled diacetate fibers [J]. Journal of Textile Research, 2024, 45(09): 42-49.
[10] CHENG Xianwei, LIU Yawen, GUAN Jinping, CHEN Rui. Preparation and flame-retardant performance of coated polyamide 6 fabrics with biomass phytic acid modified polyurethane [J]. Journal of Textile Research, 2024, 45(06): 120-126.
[11] ZHENG Xiaodi, SHENG Pinghou, JIANG Jiacen, LI Rui, JIAO Hongjuan, QIU Zhicheng. Preparation and performance of copper modified antimicrobial and anti-mite polyamide 6 fiber [J]. Journal of Textile Research, 2024, 45(03): 19-27.
[12] CHEN Jiangping, GUO Chaoyang, ZHANG Qijun, WU Renxiang, ZHONG Lubin, ZHENG Yuming. Preparation and air filtration performance of electrospun polyamide 6/polystyrene composite membranes [J]. Journal of Textile Research, 2024, 45(01): 56-64.
[13] FAN Shuo, YANG Peng, ZENG Jinhao, SONG Xiaodi, GONG Yudan, XIAO Yao. Preparation of multi-component organic polysiloxane for flame retardancy of polyamide 6 fabrics with anti-dripping behavior [J]. Journal of Textile Research, 2024, 45(01): 152-160.
[14] FAN Mengjing, WU Lingya, ZHOU Xinru, HONG Jianhan, HAN Xiao, WANG Jian. Construction of capacitive sensor based on silver coated polyamide 6/polyamide 6 nanofiber core-spun yarn [J]. Journal of Textile Research, 2023, 44(11): 67-73.
[15] LI Xiutian, SONG Weiguang, ZHANG Liping, DU Changsen, FU Shaohai. Preparation and properties of masterbatch for polyamide dope dyeing [J]. Journal of Textile Research, 2023, 44(11): 45-51.
Viewed
Full text


Abstract

Cited

  Shared   
  Discussed   
No Suggested Reading articles found!